英语翻译Twenty-four standard cylinders (150 x300 ram) were cast with each pour and tested frequently to monitor concrete strength with age.那一整段是The concrete compressive strength for the ready-mix concrete varies from 25 MPa to 62 MPa.Th

来源:学生作业帮助网 编辑:作业帮 时间:2024/05/11 17:50:38
英语翻译Twenty-four standard cylinders (150 x300 ram) were cast with each pour and tested frequently to monitor concrete strength with age.那一整段是The concrete compressive strength for the ready-mix concrete varies from 25 MPa to 62 MPa.Th

英语翻译Twenty-four standard cylinders (150 x300 ram) were cast with each pour and tested frequently to monitor concrete strength with age.那一整段是The concrete compressive strength for the ready-mix concrete varies from 25 MPa to 62 MPa.Th
英语翻译
Twenty-four standard cylinders (150 x300 ram) were cast with each pour and tested frequently to monitor concrete strength with age.
那一整段是
The concrete compressive strength for the ready-mix concrete varies from 25 MPa to 62 MPa.The slump was 250 mm to produce high performance concrete for all the specimens.Twenty-four standard cylinders (150 x 300 mm) were cast with each pour and tested frequently to monitor concrete strength with age.The compressive strength of the concrete used in each specimen is shown in Table 1.The nominal maximum size of the coarse aggregate was 10 mm diameter.

英语翻译Twenty-four standard cylinders (150 x300 ram) were cast with each pour and tested frequently to monitor concrete strength with age.那一整段是The concrete compressive strength for the ready-mix concrete varies from 25 MPa to 62 MPa.Th
每次倾倒生产24个标准圆筒(150 x300ram),所有圆筒都会经过频繁检测来监视其随着时间流逝在混凝土强度方面发生的变化
仅供参考,欢迎指正